Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Internal mold release. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is halogen free.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | TM R050-16 |
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
Eastman Eastar GN125 Copolyester, Natural
(discontinued **) Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced co.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+GF20%, General PurposeApplication: HMID, SLMP B, HolderCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Specific Gravity | 1.30 - 1.35 g/cc @Thickness 1.57 mm |
1.30 - 1.35 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP605 Paper Base Laminate Description: A paper-base laminate with low phenolic resin content for hard, flat surfaces. This material is normally used in the printed circuit board industry as a backup for the drilling operatio.. |
|||
Specific Gravity | 1.30 - 1.40 g/cc @Thickness 1.57 mm |
1.30 - 1.40 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP660 Paper Base Laminate Description: Lower cost paper phenolic NEMA Grade XP. Uses natural kraft paper without pigmented cover sheet. Warm to hot punching. UL listed. Thickness Tested: 0.062", 0.125" & 0.500" |
|||
Specific Gravity | 1.30 - 1.50 g/cc | 1.30 - 1.50 g/cc | ASTM D 792 |
Karina 804-48/1-CRE Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.30 - 1.38 g/cc | 1.30 - 1.38 g/cc | ASTM D792 |
Spartech Royalite R52 PVC/Acrylic Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | |
Shin-Etsu Silicones KMP-590 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | 23°C; ASTM D792 |
Teknor Apex APEX® 94-A0098A-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
Samyang Trirex® SF3200GNH20 Polycarbonate, Reinforced Non Halogen for Printers PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.SF3200GNH20 is a reinforced, non-halogen grade for Printers.Applications: Office Machi.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP 40% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Asia Pacific) 40% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | D792 |
Ensinger Tecapeek® ST PolyEtherKetoneEtherKetoneKetone, Unreinforced TECAPEEK® ST is a multipurpose semi-crystaline material from the polyaryletherketone family based on PEKEKK that features improved mechanical properties at higher temperatures. The benefits of TECA.. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF CP 206 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.40 g/cc | 1.30 - 1.40 g/cc | IEC 1212-2 8.1 |
Hippe PF WV 304 Wood veneer Reinforced Phenolic Resin - Sheet Parallel plied. Used in mechanical and electrical applications.Information provided by Hippe. |
|||
Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom BD-330699 PVC Compound The polycom BD series are compounds for blow molding of PVC bottles suitable for the packaging of edible oil, water, cleaning products and lubricants. These compounds produce bottles with high clar.. |
|||
Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
Axiall 17890 Wire & Cable Flexible PVC Non-lead stabilized insulation compound recommended for THW and 90C Class 43 applications. UL recognized component for THW and TW.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp.. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | Silicone Property; Arlon SQA-TMS-024 |
Arlon 54B12R006 Silicone Rubber/Fiberglass Laminate Cured silicone rubber with a fiberglass substrate. |
|||
Specific Gravity | 1.30 - 1.34 g/cc | 1.30 - 1.34 g/cc | ASTM D-792 |
Axiall 10701 Wire & Cable Flexible PVC General purpose 80°C compound with good low temperature properties recommended for 15 mil wall and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Rigid Molding M4910 (USP CLASS VI for TRANS 9494 only) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Specific Gravity | 1.30 g/cc | 1.30 g/cc | |
Gharda Chemicals G-PAEK™ 1200P Ultra High Performance PEK Polymer Product Details: Ultra High performance thermoplastic material, unreinforced Poly Aryl Ether Ketone (G-PAEK), semi-crystalline, coarse powder for extrusion compounding, FDA food contact compliant, .. |