Hippe PF WV 304 Wood veneer Reinforced Phenolic Resin - Sheet

Category Polymer , Thermoset , Phenolic
Manufacturer Erhard Hippe KG
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe PF WV 304 Wood veneer Reinforced Phenolic Resin - Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Parallel plied. Used in mechanical and electrical applications.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.40 g/cc
1.30 - 1.40 g/cc
IEC 1212-2 8.1
Mechanical Properties Metric English Comments
Tensile Strength >= 120 MPa
>= 17400 psi
IEC 1212-2 5.7
Flexural Strength >= 170 MPa
>= 24700 psi
Perpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 18.0 GPa
>= 2610 ksi
IEC 1212-2 5.2
Compressive Strength >= 80.0 MPa
>= 11600 psi
Perpendicular to laminations; IEC 1212-2 5.3
Shear Strength >= 15.0 MPa
>= 2180 psi
Parallel to laminations; IEC 1212-2 5.6
Charpy Impact Unnotched >= 2.50 J/cm²
>= 11.9 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.2
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+8 ohm
>= 1.00e+8 ohm
After immersion in water; IEC 1212-2 6.3
Dielectric Breakdown >= 25000 V

@Temperature 90.0 °C
>= 25000 V

@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Dissipation Factor <= 0.10

@Frequency 48.0 - 62.0 Hz
<= 0.10

@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
Comparative Tracking Index >= 100 V
>= 100 V
IEC 1212-2 6.4
Descriptive Properties Value Comments
Thermal Endurance 120 T.I.
IEC 1212-2 7.1