Physical Properties Metric English Comments
Specific Gravity 0.579 g/cc
0.579 g/cc
ASTM D792
PolyOne Maxxam™ SY 89-21-1 Polypropylene, Unspecified (PP, Unspecified)
Maxxam ™ SY 89-21-1 is a polypropylene copolymer compound with a pre-dispersed blowing agent for up to 50% expansion. The compound offers consistent cell structure, dielectric properties, and stren..