Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.780 g/cc | 0.780 g/cc | ASTM D297 |
Parker Chomerics ParPHorm® S1945-25 Non-Conductive Form-in-Place Gasket Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Specific Gravity | 0.780 - 0.790 g/cc | 0.780 - 0.790 g/cc | |
Michelman® Topaz Indicator Solution Description: Indicator solution for Topaz primed sheet substratesUsage: Topaz Indicator is designed to measure the uniformity of the coated substrate.Application data: 1. Soak a cotton pad with Topa.. |
|||
Specific Gravity | 0.780 g/cc | 0.780 g/cc | |
Chesterton 274 Industrial Degreaser Description: Chesterton® 274 Industrial Degreaser is an industrial strength, hard surface degreaser which will dissolve grease, oil, tar and other similar water insoluble soils generally encountere.. |
|||
Specific Gravity | 0.780 g/cc @Temperature 25.0 °C |
0.780 g/cc @Temperature 77.0 °F |
|
Dow Corning OS-2 SILICONE CLEANER & SURFACE PREP Non Ozone depleting, VOC exempt, Silicone cleaner to clean Plastic and Metals, excellent for removing oils, silicone-based car wax and protectants.Information provided by Dow Corning |
|||
Specific Gravity | 0.780 g/cc | 0.780 g/cc | |
BCC Products BC 7020 Epoxy Backfill System BC 7020 is a lightweight two component epoxy backfill system. Unlike BC 7010, the filler portion is pre-blended into the resin and hardener components for easier handling, thus simplifying the mixin.. |
|||
Specific Gravity | 0.780 g/cc | 0.780 g/cc | ASTM-D-792-66 |
BCC Products DP-11-88 Urethane Adhesive DP-11-88 is a medium viscosity quick setting easy to use urethane adhesive. This system was specifically designed to bond together the MB2001/MB3000 Model/Tooling Board to create desired dimensions .. |
|||
Specific Gravity | 0.780 g/cc | 0.780 g/cc | |
Parker Chomerics CHO-SHIELD® 1091 Adhesion Promoter for Conductive Polyurethane Coatings Information provided by Chomerics |
|||
Specific Gravity | 0.780 g/cc | 0.780 g/cc | |
Shin-Etsu Silicones Primer 4 Elastomer Primer 4 is a primer designed for bonding platinum or peroxide cure type silicone products to metals including aluminum and various plastics.Information Provided by Shin-Etsu Silicones of America, I.. |