Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.848 g/cc | 0.848 g/cc | |
ConocoPhillips Syncon® 220 Synthetic EP Gear Oil, AGMA No. 5EP Syncon EP Plus Gear Oil is a premium quality, synthetic, extreme-pressure industrial gear lubricant developed for the lubrication of enclosed gear drives and heavily loaded plain or rolling-element .. |
|||
Specific Gravity | 0.848 g/cc | 0.848 g/cc | ASTM D792 |
PolyOne Elastamax™ XL 0141-115 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |