PolyOne Elastamax™ XL 0141-115 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Elastamax™ XL 0141-115 Styrene Butadiene Block Copolymer (SBC)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in accordance with accepted test methods. All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21 for use in the packaging of food. The listings cover many uses and restrictions may apply depending on the application. For More Information contact PolyOne.
Physical Properties Metric English Comments
Specific Gravity 0.848 g/cc
0.848 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore OO 53
53
ASTM D2240
51

@Time 10.0 sec
51

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 2.48 MPa
360 psi
510 mm/min; ASTM D412A
Tensile Strength, Yield 0.207 MPa

@Strain 300 %
30.0 psi

@Strain 300 %
510 mm/min; ASTM D412A
Tear Strength 6.30 kN/m
35.9 pli
Die C, 510 mm/min; ASTM D624
Compression Set 8.0 %

@Temperature 23.0 °C,
Time 79200 sec
8.0 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
Descriptive Properties Value Comments
Agency Ratings FDA Food Contact, Unspecified Rating
Appearance Natural Color
Features Food Contact Acceptable
General Purpose
Forms Pellets
Generic Name Styrene Butadiene Block Copolymer (SBC)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Consumer Applications
General Purpose