Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.910 g/cc | 0.910 g/cc | 23/23°C; ASTM D792 |
RheTech Products P254-01 Polypropylene Copolymer, Black Applications: Air ducts - distributionFuse panel coversSplash shieldsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Quadrant EPP Proteus® O & P Grade, Natural Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Specific Gravity | 0.910 - 0.911 g/cc @Temperature 15.6 °C |
0.910 - 0.911 g/cc @Temperature 60.0 °F |
ASTM D891 |
Fibre Glast 71 Styrene Wax #71 Styrene Wax is a 5% solution of paraffin dissolved in styrene that may be added to non waxed polyester resins and gel coats to prevent the prolonged tackiness associated with thin sections of po.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | |
Mapal Plastics Maplon Type D Polypropylene Sheet Main advantages: High clarity and medium haze, High durability, Water and chemical resistance, High heat resistance, Unlimited flex life of integral hinge, Easy to convertMain disadvantages: Low scr.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | |
LG Chemical BR 1208 Polybutadiene Polymer Description: BR1208 is high cis- 1,4 polybutadiene polymer produced by a solution polymerization process employing a stereospecific catalyst to control microstructure, molecular weight and molecular.. |
|||
Specific Gravity | 0.910 - 0.913 g/cc | 0.910 - 0.913 g/cc | ASTM D1505 |
LG Chemical SEETEC ST308 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ISO 2781 |
Kraton® G1652 E (SEBS) Linear Block Copolymer Description: Kraton G1652 E polymer is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 30% mass. It is supplied from Europe in the physical .. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D4025 |
Kraton® G1652 H (SEBS) Linear Triblock Copolymer Description: Kraton G1652 H is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Kraton® FG1901 G (SEBS) grafted with MA Description: Kraton FG1924 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form i.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM 792 |
Multibase Multi-Flex® A 5703 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Heat StabilizedOzone ResistantGeneral PurposeForms:PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D1505 |
SCG Chemicals EL-Proâ„¢ P401S Polypropylene Flat Yarn/Sheet Key Characteristics: Excellent mechanical propertiesRecommended Applications:Stretch tape for jumbo woven sheetMonofilament for rope and sheetInformation provided by SCG Chemicals |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D1505 |
SCG Chemicals EL-Proâ„¢ P600F Polypropylene Film Resin Key Characteristics:Good optical propertiesHigh productivityGood openability with 3000 ppm slip agent and 2700 ppm antiblocking agentRecommended Applications:Water quenched blown film for food and a.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D1505 |
SCG Chemicals EL-Proâ„¢ P700J Polypropylene Injection Molding Key Characteristics:High stiffnessHigh glossHigh productivityGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfa.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D1505 |
SCG Chemicals EL-Proâ„¢ P701J Polypropylene Injection Molding Key Characteristics:High stiffnessHigh glossHigh productivityGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfa.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Teknor Apex TEKBOND® 6700-45 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-2452L Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 504E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 504 is an extrusion grade olefinic thermoplastic elastomer suitable for profile extrusion or blow molding. Characteristics of this product include excellent low temperature.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Yellow P20199/2 Concentrate Based In Copolymer PP DescriptionPOLYBATCH® P20199/2 is a yellow color concentrate based in copolymer PP. This concentrate was designed to provide color in blow molding applications. POLYBATCH® P20199/2 is typically .. |
|||
Specific Gravity | 0.910 - 0.920 g/cc | 0.910 - 0.920 g/cc | |
Westlake Epolene® C-26 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed Product Description: Epolene C-26 is a maleic anhydride grafted polyethylene coupling agent for polyethylene (PE) composites. The polar functionality and molecular weight are optimized to provide ba.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Yellow P20199/2 Concentrate Based In Copolymer PP DescriptionPOLYBATCH® P20199/2 is a yellow color concentrate based in copolymer PP. This concentrate was designed to provide color in blow molding applications. POLYBATCH® P20199/2 is typically .. |
|||
Specific Gravity | 0.910 g/cc @Temperature 25.0 °C |
0.910 g/cc @Temperature 77.0 °F |
|
Dow Corning MOLYKOTE® G-0101 Rolling element bearing grease for high speed applicationInformation provided by Dow Corning |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
E-Polymers EFLEX® M500 SEBS M-series: E-FLEX M series resins are a maleic anhydride grafted (MAH) polymer concentrate designed as synthetic rubber and polyolefin manufactured by E-Polymers. It offers excellent adhesion to nyl.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Quadrant EPP Proteus® White Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYFORT™ PX 1042 Information provided by A. Schulman. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Lucent Polymers PPC-310 Polypropylene, Impact Modified Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-1875HF Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Specific Gravity | 0.910 g/cc | 0.910 g/cc | ASTM D792 |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |