Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.962 - 0.968 g/cc @Temperature 25.0 °C |
0.962 - 0.968 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ 9P-N Di Nonyl Phthalate Linear phthalate esterInformation provided by PolyOne |