Polymer Property : Specific Gravity = 0.962 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
Polymax® Maxelast® P3825 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
Polymax® Maxelast® P3870 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
Polymax® Maxelast® P3877 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
Polymax® Maxelast® P3967H TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
Polymax® Maxelast® P1935 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
Polymax® Maxelast® P1940 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
Polymax® Maxelast® P3946 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 0.962 g/cc
0.962 g/cc
20/20°C
LyondellBasell TPM Tripropylene glycol methyl ether
Information provided by Lyondell.
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM 792
Multibase Multi-Flex® A 8406 A Natural TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM 792
Multibase Multi-Flex® D 5302 ELF Black TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D1505
SCG Chemicals EL-Leneâ„¢ H5818J High Density Polyethylene Injection Molding
Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D1505
SCG Chemicals EL-Leneâ„¢ H6240B High Density Polyethylene Blow Molding
Key Characteristics:Good stiffnessGood environmental stress cracking resistance (ESCR)High compressive and impact strengthGood appearanceOdorlessSafe for food contactGood printabilityRecommended App..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
Teknor Apex Telcar® TL-102 BLK 111 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Speci..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
Total HDPE 6280 High Density Polyethylene, Injection Molding Resin
Characteristics:Excellent stiffnessExcellent surface appearanceGood warp resistanceExcellent impact resistanceASTM D 1248 - Type III, Class A, Category 3FDA CompliantApplications:Dairy cratesPallets..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
Total HDPE 6420 High Density Polyethylene, Film Resin
Polyethylene: Medium molecular weight, high density film resinCharacteristics:Excellent moisture barrier propertiesLow gelsLow taste and odorHigh stiffnessGood processabilityGood compatibility with..
Specific Gravity 0.962 g/cc
0.962 g/cc
ISO 1183
Total HDPE HD 6221 High Density Polyethylene - Blow Molding
HDPE HD 6221 is a high density polyethylene with very high stiffness and impact resistance. The low viscosity of this grade has been designed for the manufacture of thin walled containers for foods..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
Total HDPE 6480 High Density Polyethylene, Clarity Cast Film Resin
Polyethylene: Clarity High Density Cast Film ResinCharacteristics:High stiffnessHigh clarityExcellent surface glossHigh tensile strengthGood barrier propertiesLow gel contentApplications:OverwrapFo..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D1505
Chevron Phillips Marlex® 9519H High Density Polyethylene, Blow Molding
This gas phase, high molecular weight, homopolymer with antistatic agent is tailored for lightweight blow molded applications that:Require excellent stiffness to ESCR ratioRequire good melt strength..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
Teknor Apex Sinelec CCB6814 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Uses: Corrugated Sheet Forms: Pellets Processing Method: Injection Method; Sheet Extr..
Specific Gravity 0.962 - 0.968 g/cc

@Temperature 25.0 °C
0.962 - 0.968 g/cc

@Temperature 77.0 °F
ASTM D4052
PolyOne Synplast™ 9P-N Di Nonyl Phthalate
Linear phthalate esterInformation provided by PolyOne
Specific Gravity 0.962 g/cc
0.962 g/cc
Radici Radilene® R 70 IE 0 2060 C High Density Polyethylene
Shore hardness: 61 D (3s)Processable, recyclable, no charge and completely non-toxicApplication examples: coating of corrugated and non-corrugated pipe (conduit, plumbing pipe, steel pipe coating a..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D1505
SCG Chemicals EL-Lene™ H6140B High Density Polyethylene Blow Molding
Key Characteristics:Good processabilityHigh stiffnessGood environmental stress cracking resistance (ESCR)High compressive and impact strengthExcellent appearanceOdorlessSafe for food contactGood pri..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
Braskem Green PE SGF4960 Blow Molding and Monofilament High Density Polyethylene
Description: SGF4960 is a homopolymer high-density polyethylene, developed for the blow-molding segment with high density and stiffness combined with high impact resistance. The minimum biobased con..
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D1505
Chevron Phillips Marlex® 9518H High Density Polyethylene, Blow Molding
This gas phase, high molecular weight, homopolymer is tailored for lightweight blow molded applications that:Require excellent stiffness to ESCR ratioRequire good melt strengthAre durable and recycl..