Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.19 - 1.25 g/cc | 1.19 - 1.25 g/cc | ASTM D 792 |
Karina E600D06/958 Light Blue PVC Compound Shoe IndustryInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.15 - 1.25 g/cc | 1.15 - 1.25 g/cc | ASTM D792 |
Loxim 830 02T V0 Polypropylene Compound, 30% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Specific Gravity | 1.15 - 1.25 g/cc | 1.15 - 1.25 g/cc | BAM 1014 |
Kraton® G7705 GI-B (SEBS) Compound Description: Kraton G7705 GI-B is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Specific Gravity | 1.15 - 1.25 g/cc | 1.15 - 1.25 g/cc | BAM 1014 |
Kraton® G7705 GI-N (SEBS) Compound Description: Kraton G7705 GI-N is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Specific Gravity | 1.19 - 1.25 g/cc | 1.19 - 1.25 g/cc | ASTM D 792 |
Karina 02/127-FC-LMP Yellow Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.19 - 1.25 g/cc | 1.19 - 1.25 g/cc | ASTM D 792 |
Karina 608-48/1-Y-IS-BZ Black PVC Compound Heavy metal free, weather resistant PVC Compound; recommended for injection and extrusion of automotive profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.21 - 1.25 g/cc | 1.21 - 1.25 g/cc | ASTM D 792 |
Karina 65/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.21 - 1.25 g/cc | 1.21 - 1.25 g/cc | ASTM D 792 |
Karina 650D48/1-A-IS-BZ Black PVC Compound Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.21 - 1.25 g/cc | 1.21 - 1.25 g/cc | ASTM D 792 |
Karina 700D48/1-IS Black PVC Compound PVC Compound recommended for automotive parts injection. Also recommended for retractable telephone wire sheeting.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.19 - 1.25 g/cc | 1.19 - 1.25 g/cc | ASTM D 792 |
Karina E 02/127-FC-LMP Yellow Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.19 - 1.25 g/cc | 1.19 - 1.25 g/cc | ASTM D 792 |
Karina E 27/8-GIN Fume MBATCH (SP31452) for PVC Recommended usage from 2% to 3% on crystal PVC compound (kind of gray for crystal)Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.19 - 1.25 g/cc | 1.19 - 1.25 g/cc | ASTM D 792 |
Karina E 42/231-GE Red MBATCH for PVC Recommended usage from 2% to 3% on crystal PVC compound (transparent red)Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.19 - 1.25 g/cc | 1.19 - 1.25 g/cc | ASTM D 792 |
Karina E 601D22/15 Crepe PVC Compound For footware/soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.21 - 1.25 g/cc | 1.21 - 1.25 g/cc | ASTM D 792 |
Karina 600D18/136-A-IS-BZ Gray PVC Compound Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.18 - 1.25 g/cc | 1.18 - 1.25 g/cc | ASTM D792 |
Spartech Royalite R59 ABS/PVC Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.18 - 1.25 g/cc | 1.18 - 1.25 g/cc | ASTM D792 |
Spartech Royalite R87/59 ABS/PVC Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.20 - 1.25 g/cc | 1.20 - 1.25 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Specific Gravity | 1.20 - 1.25 g/cc | 1.20 - 1.25 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Specific Gravity | 1.20 - 1.25 g/cc | 1.20 - 1.25 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Specific Gravity | 1.20 - 1.25 g/cc | 1.20 - 1.25 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Specific Gravity | 1.20 - 1.25 g/cc | 1.20 - 1.25 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Specific Gravity | 1.21 - 1.25 g/cc | 1.21 - 1.25 g/cc | ASTM D-792 |
Axiall 6704 Moldings & Extrusions Flexible PVC An expandable, low gravity, injection molding compound specifically developed for footwear applications. Finished product appearance is matte, similar to TPR.Information provided by Georgia GulfGeo.. |
|||
Specific Gravity | 1.21 - 1.25 g/cc | 1.21 - 1.25 g/cc | ASTM D-792 |
Axiall 8602 Moldings & Extrusions Flexible PVC A vinyl elastomer extrusion compound with rubber-like properties. Ideally suited for extruded profiles, tubings and co-extruded shapes.Information provided by Georgia GulfGeorgia Gulf became Axiall.. |
|||
Specific Gravity | 1.21 - 1.25 g/cc | 1.21 - 1.25 g/cc | ASTM D-792 |
Axiall 8833 Moldings & Extrusions Flexible PVC A clear, flexible PVC compound best suited for 80C automotive tubing applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.21 - 1.25 g/cc | 1.21 - 1.25 g/cc | ASTM D-792 |
Axiall 10753 Wire & Cable Flexible PVC Flame retardant 60C compound suitable for integral non-metallic conduit and general purpose jacket applications. Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.21 - 1.25 g/cc | 1.21 - 1.25 g/cc | ASTM D-792 |
Axiall 6730 Moldings & Extrusions Flexible PVC Injection molding compound with good processing characteristics that allow fast cycles and smooth unblemished surfaces on the finished product. Exhibits good weathering and low temperature properti.. |
|||
Specific Gravity | 1.21 - 1.25 g/cc | 1.21 - 1.25 g/cc | ASTM D-792 |
Axiall 8872 Moldings & Extrusions Flexible PVC A clear extrusion and molding grade compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.21 - 1.25 g/cc | 1.21 - 1.25 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom VY-310585 PVC Compound The Polycom VY series are compounds for the extrusion of both stripes for chaise lounge and flexible window sidings with outstanding weather and outdoors resistance. Also, in the VY series the are .. |
|||
Specific Gravity | 1.20 - 1.25 g/cc | 1.20 - 1.25 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Specific Gravity | 1.21 - 1.25 g/cc | 1.21 - 1.25 g/cc | ASTM D-792 |
Axiall 38901 Wire & Cable Flexible PVC Non-lead flame retardant flexible PVC compound suitable for integral conduit jackets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |