Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.66 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Ovation Polymers Nemcon™ H ABS DP116P ABS
ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Celanese Celanex® 3316 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3316 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/16 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
RTP Company RTP 1107  Polyethylene Terephthalate (PET) Glass Fiber 40%  (discontinued **)<
Glass Fiber 40%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Celanese FORTRON 1140L7 PPS, 40% Glass Reinforced  (Unverified Data**)
One of the easiest flowing 40% glass reinforced grade in the Fortron product line. This material can be processed at fast cycle times due to the unique crystallization characteristics. This product ..
Specific Gravity 1.66 g/cc

@Temperature 25.0 °C
1.66 g/cc

@Temperature 77.0 °F
STM 2
Lord Adhesives Thermosetâ„¢ SC-309 Thermally Conductive Silicone Encapsulating System
Lord SC-309 is a two part thermally conductive silicone system with a convenient 1:1 by weight or volume mix ratio.Lord SC-309 cures to a flexible elastomer, which offers the low stress characterist..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
LG Chemical Lupox® GP2306FY PBT+GF30%
Description: Injection Molding, PBT+GF30%Flame Retardant, GWITApplication: IT/OA, E&E (Connector)CAS No. 88497-56-7, 65997-17-3, 37640-57-6, 24968-12-5, 25038-59-9 and 1309-64-4Information provided ..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D 792
SABIC Innovative Plastics Ultem 3451 PEI
45% Glass fiber and mineral filled, standard flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East)
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
Specific Gravity 1.66 g/cc
1.66 g/cc
Silberline EternaBrite® Premier 251-PA
EternaBrite® Premier pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on lenticular flake geometry and offer enhanced leafing properties in solven..
Specific Gravity 1.66 g/cc
1.66 g/cc
Silberline Sparkle Silvex® 963-30-C
Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited ..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow LL20203/2 Concentrate Based In LDPE
DescriptionPOLYBATCH® LL20203/2 is a yellow color concentrate based in LDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL20203/2 is typi..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D 792
RTP Company RTP 1305 TFE 13 SI 2 Polyphenylene Sulfide (PPS), Glass Fiber Reinforced - PTFE & Silicone Lubricated
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow LL20203/2 Concentrate Based In LDPE
DescriptionPOLYBATCH® LL20203/2 is a yellow color concentrate based in LDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL20203/2 is typi..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D 792
RTP Company RTP 2309 C Rigid Thermoplastic Polyurethane (RTPU), Glass Fiber
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
A. Schulman POLYBATCH™ Grey 8760 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 8760 is a grey color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 8..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
A. Schulman POLYBATCH™ Grey 8760 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 8760 is a grey color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 8..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow LL20203/2 Concentrate Based In LDPE
DescriptionPOLYBATCH® LL20203/2 is a yellow color concentrate based in LDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL20203/2 is typi..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Lubrizol ESTALOC® 59600 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro..
Specific Gravity 1.66 g/cc
1.66 g/cc
Part A
Epoxy Technology EPO-TEK® 930 Thermally Conductive Epoxy
Material Description: A two-part thermally conductive epoxy for heat sinking electronics and hybrids. It can be used at the PCB level for circuit assembly.Information Provided by Epoxy Technology
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
Specific Gravity 1.66 g/cc
1.66 g/cc
BYK Cloisite® 15A Nanoclay
Cloisite® 15A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr..
Specific Gravity 1.66 g/cc
1.66 g/cc
Aremco Aremco-Bond™ 805 Thermally Conductive Material, Aluminum Filled
Thermally Conductive, Aluminum-Filled, Two-Part Epoxy Paste. Low Shrink Rate & Excellent Mechanical Strength to 570 ºF.
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Celanese CELANEX 3316 PBT, 30% Glass Reinforced
Celanex 3316 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/16 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan..
Specific Gravity 1.66 g/cc
1.66 g/cc
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, Jet Black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, s..
Specific Gravity 1.66 g/cc
1.66 g/cc
Aremco Ceramacoat™ 845-GLT High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, light-green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps,..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
E-Polymers SEPAZ® V330FR 30% Glass Fiber Reinforced Flame Retardant PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow LL20203/2 Concentrate Based In LDPE
DescriptionPOLYBATCH® LL20203/2 is a yellow color concentrate based in LDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL20203/2 is typi..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
RTP Company RTP 4005A FR  Polyphthalamide - Hot Water Mold (PPA) Glass Fiber 30% - Flame Retardant &a
Glass Fiber 30% - Flame RetardantComments:Glass FiberFlame RetardantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information ..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Celanese FORTRON 11400000000 PPS, 40% Glass Reinforced  (Unverified Data**)
Fortron 1140E7 is an inherently flame-retardant grade exhibiting extremely low flash and fast cycle times. It has excellent electrical properties, high hardness and stiffness. This grade exhibits go..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Oxford Polymers 30GF-25PTFE 30% Glass Fiber/PTFE Reinforced Polyphenylene Sulfide  (discontinued **)
30% Glass Fiber/PTFE Reinforced Polyphenylene SulfideInformation provided by Oxford Polymers.