Polymer Property : Specific Gravity = 1.66 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D 792
RTP Company RTP 4000 AS-1551 HS Polyphthalamide (PPA), Mineral - Glass Fiber
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced  (Unverified Data**)
Fortron 1140L4 is a 40% glass-reinforced grade that is the strongest and toughest product available. It exhibits excellent heat and chemical resistance, good electrical properties and is inherently ..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Celanese FORTRON 1140L7 PPS, 40% Glass Reinforced  (Unverified Data**)
One of the easiest flowing 40% glass reinforced grade in the Fortron product line. This material can be processed at fast cycle times due to the unique crystallization characteristics. This product ..
Specific Gravity 1.66 g/cc

@Temperature 25.0 °C
1.66 g/cc

@Temperature 77.0 °F
STM 2
Lord Adhesives Thermosetâ„¢ SC-309 Thermally Conductive Silicone Encapsulating System
Lord SC-309 is a two part thermally conductive silicone system with a convenient 1:1 by weight or volume mix ratio.Lord SC-309 cures to a flexible elastomer, which offers the low stress characterist..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D 792
SABIC Innovative Plastics Ultem 3451 PEI
45% Glass fiber and mineral filled, standard flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D 792
SABIC Innovative Plastics Ultem 3451 PEI (Asia Pacific)
45% Glass fiber and mineral filled, standard flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East)
Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell..
Specific Gravity 1.66 g/cc
1.66 g/cc
Shin-Etsu Silicones KEP-12 Silicone additive
KEP12 is an additive which can be used in most of the silicone products to improve heat stability.Product Features: Improve thermal stability and compression set.Excellent dispersion.Information Pro..
Specific Gravity 1.66 g/cc
1.66 g/cc
Silberline EternaBrite® Premier 251-PA
EternaBrite® Premier pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on lenticular flake geometry and offer enhanced leafing properties in solven..
Specific Gravity 1.66 g/cc
1.66 g/cc
Silberline Sparkle Silvex® 963-30-C
Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited ..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Samsung Cheil Industries Infino® XP-2140C PPS
Information provided by Samsung Cheil Industries.
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp WB008 PBT
LNP* Thermocomp* WB008 is a compound based on Thermoplastic Polyester (PBT) containing Glass Beads.This data was supplied by SABIC-IP for the Americas region.
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
A. Schulman POLYBATCH™ Grey 8760 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 8760 is a grey color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 8..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow LL20203/2 Concentrate Based In LDPE
DescriptionPOLYBATCH® LL20203/2 is a yellow color concentrate based in LDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL20203/2 is typi..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D 792
RTP Company RTP 2000 B-340 Polysulfone Alloy, Glass Fiber
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D 792
RTP Company RTP 2309 C Rigid Thermoplastic Polyurethane (RTPU), Glass Fiber
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow LL20203/2 Concentrate Based In LDPE
DescriptionPOLYBATCH® LL20203/2 is a yellow color concentrate based in LDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL20203/2 is typi..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
A. Schulman POLYBATCH™ Grey 8760 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 8760 is a grey color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 8..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D 792
RTP Company RTP 205 FR Nylon 6/6 (PA), Glass Fiber - Flame Retardant - UL94 V-0
The RTP series of flame retardant, glass fiber reinforced nylon materials are designed to provide the optimal balance of strength, electrical and ignition resistance properties while exhibiting exce..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Lubrizol ESTALOC® 59600 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro..
Specific Gravity 1.66 g/cc
1.66 g/cc
Part A
Epoxy Technology EPO-TEK® 930 Thermally Conductive Epoxy
Material Description: A two-part thermally conductive epoxy for heat sinking electronics and hybrids. It can be used at the PCB level for circuit assembly.Information Provided by Epoxy Technology
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Data provided by Clariant Masterbatches
Specific Gravity 1.66 g/cc
1.66 g/cc
Aremco Aremco-Bond™ 805 Thermally Conductive Material, Aluminum Filled
Thermally Conductive, Aluminum-Filled, Two-Part Epoxy Paste. Low Shrink Rate & Excellent Mechanical Strength to 570 ºF.
Specific Gravity 1.66 g/cc
1.66 g/cc
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, Jet Black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, s..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
RTP Company RTP 3285  Ethylene Tetrafluoroethylene (ETFE) Carbon Fiber 30%  (discontinued **
Carbon Fiber 30%Comments:Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
A. Schulman POLYBATCH™ Yellow LL20203/2 Concentrate Based In LDPE
DescriptionPOLYBATCH® LL20203/2 is a yellow color concentrate based in LDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL20203/2 is typi..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
E-Polymers SEPAZ® C130HS 30% Glass Fiber Reinforced High Temperature Stabilized LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Celanese FORTRON 11400000000 PPS, 40% Glass Reinforced  (Unverified Data**)
Fortron 1140E7 is an inherently flame-retardant grade exhibiting extremely low flash and fast cycle times. It has excellent electrical properties, high hardness and stiffness. This grade exhibits go..