Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.82 g/cc | 1.82 g/cc | ASTM D792 |
PolyOne Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Specific Gravity | 1.82 g/cc | 1.82 g/cc | ASTM D792 |
Quantum Composites HTC-9500 55% E-Glass Fiber Reinforced Bismaleimide SMC, High Temperature Composite HTC-9500 (127-51-6) is an E-Glass Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristics providing .. |
|||
Specific Gravity | 1.82 g/cc | 1.82 g/cc | ASTM D792 |
Quantum Composites LYTEX® 4129 63% Glass Fiber Reinforced Epoxy SMC LYTEX 4129 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention .. |
|||
Specific Gravity | 1.82 g/cc | 1.82 g/cc | ASTM D792 |
Quantum Composites QC-2150 50% Glass Reinforced Phenolic SMC QC-2150 is a glass reinforced phenolic engineered structural composite molding compound. It exhibits outstanding low flammability characteristics. QC-2150 is recommended for applications such as a.. |
|||
Specific Gravity | 1.82 g/cc | 1.82 g/cc | ASTM D792 |
Noble Polymers Ecobarrier™ 0918 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Specific Gravity | 1.82 g/cc | 1.82 g/cc | |
Premix Premi-Glas® 1286 Glass Reinforced SMC Description: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression molding.. |
|||
Specific Gravity | 1.82 g/cc | 1.82 g/cc | ASTM D792 |
PolyOne Therma-Tech™ SF-6000 TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Specific Gravity | 1.82 g/cc | 1.82 g/cc | ASTM D297 |
Greene Tweed Fluoroelastomer 742 FKM Fluoroelastomer 742 performs well in aggressive chemicals and where ultrapure materials are not required. Recommended for conventional wet and dry system applications, Fluoroelastomer 742 has a goo.. |
|||
Specific Gravity | 1.82 g/cc | 1.82 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7327 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Specific Gravity | 1.82 g/cc | 1.82 g/cc | ASTM D297, 15 |
Seals Eastern 7265D Fluorocarbon-Elastomer Formulated Viton-ETP®. High temperature service in aggressive chemicals; Good base resistance.Information provided by Seals Eastern, Inc. |
|||
Specific Gravity | 1.82 g/cc | 1.82 g/cc | |
Silberline Aquasil® "BP" 3622 Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and .. |
|||
Specific Gravity | 1.82 - 1.88 g/cc | 1.82 - 1.88 g/cc | |
Bulk Molding Compounds BMC 1423 Wear Resistant, Electrical Grade BMC 1423 is a wear-resistant electrical grade material used in applications where there are moving parts. Best anti-wear properties are exhibited when used in conjunction with mating parts molded fr.. |
|||
Specific Gravity | 1.82 g/cc | 1.82 g/cc | ASTM D792 |
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC thermosets are the most .. |
|||
Specific Gravity | 1.82 g/cc | 1.82 g/cc | ASTM D792 |
PolyOne Synprene® IT 37-023 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:General PurposeMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation .. |