Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.84 - 1.88 g/cc | 1.84 - 1.88 g/cc | ASTM D792 |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Specific Gravity | 1.82 - 1.88 g/cc | 1.82 - 1.88 g/cc | |
Bulk Molding Compounds BMC 1423 Wear Resistant, Electrical Grade BMC 1423 is a wear-resistant electrical grade material used in applications where there are moving parts. Best anti-wear properties are exhibited when used in conjunction with mating parts molded fr.. |