Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.93 - 1.98 g/cc | 1.93 - 1.98 g/cc | ISO 1183 |
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very .. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvet® 220-20-E Silvet® E grades are economical aluminum pigments provided in pellet form for easy handling and incorporation. They are composed of 80% aluminum pigment and 20% polyolefin and are compatible with.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvet® 420-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvet® 430-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvet® 440-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvex® 113-20-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvex® 333-20-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvex® 335-20-D Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Sparkle Silvex® Premier 860-20-D Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvet® 460-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvet® 540-20-E Silvet® E grades are economical aluminum pigments provided in pellet form for easy handling and incorporation. They are composed of 80% aluminum pigment and 20% polyolefin and are compatible with.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvex® 543-20-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Sparkle Silvex® Premier 838-20-D Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 AP is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 MG is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8844 GP DescriptionPOLYBATCH® LL8844 GP is a general purpose white color concentrate containing 45% TiO2 based in LLDPE. This product has been designed to provide color and opacity with good dispersion an.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 AP is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 MG is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8844 GP DescriptionPOLYBATCH® LL8844 GP is a general purpose white color concentrate containing 45% TiO2 based in LLDPE. This product has been designed to provide color and opacity with good dispersion an.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 MG is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 MG is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8844 GP DescriptionPOLYBATCH® LL8844 GP is a general purpose white color concentrate containing 45% TiO2 based in LLDPE. This product has been designed to provide color and opacity with good dispersion an.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 AP is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Bulk Molding Compounds BMC 6241 Glass Fiber Reinforced Compound BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availabl.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Bulk Molding Compounds BMC 610 Mineral Filled, Glass Reinforced Polyester Compound BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Sparkle Silvet® 790-20-E Sparkle Silvet® E grades are economical aluminum pigments provided in pellet form for easy handling and incorporation. They are composed of 80% aluminum pigment and 20% polyolefin and are compatibl.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 MG is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8844 GP DescriptionPOLYBATCH® LL8844 GP is a general purpose white color concentrate containing 45% TiO2 based in LLDPE. This product has been designed to provide color and opacity with good dispersion an.. |