Polymer Property : Specific Gravity = 2.23 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.13 - 2.23 g/cc
2.13 - 2.23 g/cc
ASTM D1457-18; ISO.1183 DN.53479
Polimersan Plastics POLITEF® (PTFE)
POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of ..
Specific Gravity 2.13 - 2.23 g/cc
2.13 - 2.23 g/cc
ASTM D1457-18; ISO.1183 DN.53479
Polimersan Plastics POLITEF® (PTFE)
POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of ..
Specific Gravity 2.17 - 2.23 g/cc
2.17 - 2.23 g/cc
ASTM D 792
Karina 1000/2065-IE MBPEB White (DT) Color Concentrate
Filled white color concentrate recommended for polyolefins applications.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 2.17 - 2.23 g/cc
2.17 - 2.23 g/cc
ASTM D 792
Karina E 1000/3055-IE MBPEB White Color Concentrate
TIO2+ mineral concentrate recommended for polyolefins application (films, packaging, bags, etc.).Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 2.20 - 2.23 g/cc
2.20 - 2.23 g/cc
ASTM D792
Adamas Adalon® 209 PTFE, 15% Glass Filled
Information provided by Adamas, HPM
Specific Gravity 2.20 - 2.23 g/cc
2.20 - 2.23 g/cc
ASTM D792
Adamas Adalon® 215 PTFE, 17% Glass Filled, Blue
Information provided by Adamas, HPM
Specific Gravity 2.21 - 2.23 g/cc
2.21 - 2.23 g/cc
ASTM D792
Adamas Adalon® 252 PTFE, 28% Glass Fiber
Information provided by Adamas, HPM
Specific Gravity 2.21 - 2.23 g/cc
2.21 - 2.23 g/cc
ASTM D792
Adamas Adalon® 254 PTFE, 28% Glass Fiber
Information provided by Adamas, HPM