Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.74 - 2.26 g/cc | 1.74 - 2.26 g/cc | ASTM D792 |
Parker Chomerics Tecknit Consil®-A 895 Silver-Aluminum Filled Silicone Elastomer Description: CONSIL-A is a silicone or fluorosilicone elastomer filled with silver-plated aluminum particles designed to achieve maximum electrical conductivity. CONSIL-A provides high shielding eff.. |
|||
Specific Gravity | 1.74 - 2.26 g/cc | 1.74 - 2.26 g/cc | ASTM D792 |
Parker Chomerics Tecknit Consil®-A 897 Silver-Aluminum Filled Silicone Elastomer Description: CONSIL-A is a silicone or fluorosilicone elastomer filled with silver-plated aluminum particles designed to achieve maximum electrical conductivity. CONSIL-A provides high shielding eff.. |
|||
Specific Gravity | 1.74 - 2.26 g/cc | 1.74 - 2.26 g/cc | ASTM D792 |
Parker Chomerics Tecknit NC-Consil® 750 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Specific Gravity | 1.74 - 2.26 g/cc | 1.74 - 2.26 g/cc | ASTM D792 |
Parker Chomerics Tecknit NC-Consil® 751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Specific Gravity | 1.74 - 2.26 g/cc | 1.74 - 2.26 g/cc | ASTM D792 |
Parker Chomerics Tecknit NC-Consil® 770 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Specific Gravity | 1.74 - 2.26 g/cc | 1.74 - 2.26 g/cc | ASTM D792 |
Parker Chomerics Tecknit NC-Consil® FR751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Specific Gravity | 2.23 - 2.26 g/cc | 2.23 - 2.26 g/cc | ASTM D792 |
Isoflon PTFE + 25% Glass Polytetrafluoroethylene with 25% Glass Properties:Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityApplications: Dynamic seals with rotating or alternating motion.Information provided by Iso.. |
|||
Specific Gravity | 2.22 - 2.26 g/cc | 2.22 - 2.26 g/cc | ASTM D792 |
Isoflon PTFE +28% GL Blue-E glass-1% Blue Polytetrafluoroethylene with 28% GL-Blue-E glass-1% Blue (equivalent VX1) Properties:Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityInformation provided by Isoflon. |