Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Isoflon PTFE + 25% Glass Polytetrafluoroethylene with 25% Glass

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer Isoflon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon PTFE + 25% Glass Polytetrafluoroethylene with 25% Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties:Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityApplications: Dynamic seals with rotating or alternating motion.Information provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 2.23 - 2.26 g/cc
2.23 - 2.26 g/cc
ASTM D792
Deformation 5.0 - 6.0 %

@Time 86400 sec
5.0 - 6.0 %

@Time 24.0 hour
Permanent, after Relaxation; ASTM D695
10 - 12 %

@Pressure 0.0000140 MPa,
Time 86400 sec
10 - 12 %

@Pressure 0.00203 psi,
Time 24.0 hour
Under Load; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 60 - 65
60 - 65
ASTM D2240
Tensile Strength 13.0 - 18.0 MPa
1890 - 2610 psi
ASTM D4894
Elongation at Break 180 - 220 %
180 - 220 %
ASTM D4894
Coefficient of Friction, Dynamic 0.070
0.070
ASTM D1894
Thermal Properties Metric English Comments
Thermal Conductivity 0.410 W/m-K
2.85 BTU-in/hr-ft²-°F
ASTM D C177
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -200 °C
-328 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257