Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.294 g/cc | 2.294 g/cc | uncured |
Atom Adhesives AA-BOND 2156 Epoxy Adhesive AA-BOND 2156 is a thixotropic (smooth paste) thermally conductive epoxy system. It is used for staking heat sinks, transistors, diodes, resistor, integrated circuits and other heat-sensitive compone.. |