Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.41 g/cc | 2.41 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-8432 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |