Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Old Hickory APG-300 Kentucky Ball Clay This is an extremely low 325 Mesh wet residue clay. It can be employed in a variety of applications where high purity mineral filler is required. It has a moderate GE brightness value and is particu.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | ASTM D792 |
P & P Technology Nickel Graphite Loaded EPDM Molding grade conductive EPDM elastomer loaded with nickel graphite filler. The material is dark grey in color and is specially compounded to give high EMC performance and excellent IP sealing.Infor.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Alumex™ Kaolin Alumex is a Hydrated Aluminum Silicate used as a low surface area “soft†filler for Elastomeric systems.Information provided by Imerys |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Amlockâ„¢ 321 Kaolin Information provided by Imerys |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Barden™ AG-1 Kaolin Barden R is a Hydrated Aluminum Silicate available as an Air Float Beneficiated Fine Powder. This kaolin product is used as a high surface area “hard†filler for agricultural purposes.Info.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Bardenâ„¢ Kaolin Barden is a high surface area kaolin product used a filler in rubber and plastic applications.Information provided by Imerys |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Barnetâ„¢ Kaolin Information provided by Imerys |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Mercapâ„¢ 100 Kaolin Information provided by Imerys |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Imerys Minsparâ„¢ 3 Ground Feldspar Minsparâ„¢ 3 is a coarse particle size, ground Feldspar with a tightly controlled particle size distribution. The angular particle shape and inherent cheMical resistance make Minsparâ„¢ 3 an e.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | 60°C for 1,000 hrs with 90% RH; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-HFd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-HFd has a hardened top surface and mesh embedded over.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | 150°C for 1,000 hrs; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-HFd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-HFd has a hardened top surface and mesh embedded over.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | JIS-K-6220; ASTM D-792 |
Fujipoly Industries Sarcon® GR-HFd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-HFd has a hardened top surface and mesh embedded over.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin KaMin® 70C Kaolin Clay - Calcined High brightness, work-horse calcined kaolin clay, extremely low crystalline silica content.Industry: Paint & Coatings, Adhesives & SealantsUses: Architectural Coatings, Industrial Coatings, Flat/Mat.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin KaMin® 95 Kaolin Clay - Waterwashed KaMin® 95 is a medium-brightness, kaolin clay filler for paints, adhesives and related industries. It has a neutral pH, is acid-resistant and environmentally friendly.Industry: Adhesives & Sealan.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin KaMin® HG90 Kaolin Clay - Ultrafine, high brightness KaMin® HG90 is a high brightness, ultra-fine particle size, platy kaolin with moderate water demand providing good tinting strength, Ti02 extension and gloss in water based paints. KaMin® HG90.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin KaMin® Tek 2001 Clay The uniform, narrow particle size distribution and excellent color makes Kamin® TEK 2001 the preferred extender for gloss latex paints where optimum TiO2 spacing is desired without adverse effect.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Nucap® 100G Kaolin Clay - Surface Treated Cost effective, moderate brightness, mercapto silane treated clay for partial thermal black replacement.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl Rubber, EP.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyfil® XB Kaolin Clay - Waterwashed Cost effective, kaolin extender offering improved consistency vs air floated clays, spray-dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, EPDM, Wire & CableIn.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyplate® P Kaolin Clay - Delaminated Polyplate® P is a high brightness, delaminated clay intended for use in latex paints, water flexography inks, water-based adhesives or water-based systems where increased hiding, tinting strength.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | 150°C for 1,000 hrs; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-Hd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Hd has a hardened top surface.Information provided by.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | JIS-K-6220; ASTM D-792 |
Fujipoly Industries Sarcon® GR-Hd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Hd has a hardened top surface.Information provided by.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | 70°C for 1,000 hrs; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-Hd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Hd has a hardened top surface.Information provided by.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyfil® 70 Kaolin Clay - Calcined Calcined clays, such as Polyfil® 70, are brighter than most water-washed clays, offering excellent processing and limited reinforcement. They impart outstanding wet/dry electrical properties due .. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyfil® F Kaolin Clay - Waterwashed Water washed kaolin clays such as Polyfil® F offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® F is a moderate brightness water .. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyfil® FB Kaolin Clay - Waterwashed Water washed kaolin clays such as Polyfil® FB offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® FB is a moderate brightness wate.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyfil® HG Kaolin Clay - Waterwashed Polyfil® HG is an ultra-fine particle size, moderate brightness water washed kaolin clay. It offers acid resistance, barrier properties, reinforcement, neutral ph, and extremely low crystalline .. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Silberline SilBerCote® PC 3101X SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
Silberline SilBerCote® PC 8602X SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert.. |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | ASTM D792 |
Clariant Renol PPSP0006HW Polypropylene Homopolymer, Heavy Weight Compound Data provided by Clariant Masterbatches |
|||
Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
KaMin Polyfil® 35 Kaolin Clay - Waterwashed Coarse kaolin, with the lowest oil absorption, for extending without reinforcement, milled powder form.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, General Plastics, SMC/B.. |