Material Notes:
High brightness, work-horse calcined kaolin clay, extremely low crystalline silica content.Industry: Paint & Coatings, Adhesives & SealantsUses: Architectural Coatings, Industrial Coatings, Flat/Matte, Traffic Paint, Pigmented Coatings, Polyurethane, HotmeltInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Bulk Density 0.368 - 0.449 g/cc
0.0133 - 0.0162 lb/in³
Loose
Brightness 91 %
91 %
Reflectance (TAPPI)
Oil Absorption 54 %
54 %
Fineness >= 5
>= 5
Hegman Grind
Moisture Absorption at Equilibrium <= 0.5 %
<= 0.5 %
As Produced
Particle Size 1.30 µm
1.30 µm
Average Stokes Equivalent Diameter
3.20 µm
3.20 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.005% Retained
pH 6
6
100 g/250 ml H2O Slurry
Specific Surface Area 8.00 m²/g
8.00 m²/g
BET
Descriptive Properties Value Comments
Bulking Value 21.9 lb.gal
CAS Number 92704-41-1
Crystalline Silica (quartz) <0.1%
Physical Form Dry
Shipping Point Macon, GA