Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.90 g/cc | 2.90 g/cc | |
Nyco NYAD® G Special Wollastonite Wollastonite (calcium metasilicate, or CaSiO3) is a naturally occurring white, non-metallic mineral with an acicular or needle-shaped crystal structure. This distinctive property makes wollastonite .. |
|||
Specific Gravity | 2.90 g/cc | 2.90 g/cc | |
Resin Technology Group TIGA 920H Flexible Silver Conductive 100 parts resin to 115 parts hardener.TIGA 920-H is a flexible, conductive silver filled epoxy adhesive. It is recommended for bonding, and sealing electronic applications that require high flexibil.. |
|||
Specific Gravity | 2.90 g/cc | 2.90 g/cc | |
Malvern Minerals Wollastokup® FF Silane Treated Wollastonite Wollastokup® is a custom, silane treated calcium metasilicate (wollastonite) which is used as a functional filler in coatings, plastics, rubber and others due in part to its acicular or “too.. |
|||
Specific Gravity | 2.90 g/cc | 2.90 g/cc | |
Malvern Minerals Wollastokup® FT Silane Treated Wollastonite Wollastokup® is a custom, silane treated calcium metasilicate (wollastonite) which is used as a functional filler in coatings, plastics, rubber and others due in part to its acicular or “too.. |
|||
Specific Gravity | 2.90 g/cc | 2.90 g/cc | Mixed |
Tra-Con Tra-Duct 2916 Room Temperature Conductive Silver Epoxy Adhesive TRA-DUCT 2916 is an electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled with good ele.. |
|||
Specific Gravity | 2.90 g/cc | 2.90 g/cc | Mixed |
Tra-Con Tra-Duct 2916T Room Temperature Conductive Silver Epoxy Adhesive TRA-DUCT 2916T is an electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled with good el.. |
|||
Specific Gravity | 2.90 g/cc | 2.90 g/cc | |
Master Bond EP3HTS Silver Filled, Electrically Conductive Epoxy Description: Master Bond Polymer System EP3HTS is a one component, silver filled, electrically conductive epoxy system featuring high shear strength and good temperature resistance along with a fast.. |
|||
Specific Gravity | 2.90 g/cc | 2.90 g/cc | |
Aremco Pyro-Putty™ 2500 High Temperature Ceramic-Metallic Putty, Iron Oxide Filled Ceramic and Black Iron Oxide-Filled, One-Part, Water Based Paste.For Applications to 1/4" Thick.Repairs Cast Iron, and Steel Parts to 1600°F |
|||
Specific Gravity | 2.90 g/cc | 2.90 g/cc | |
Master Bond EP3HTSMed Silver Filled, Medical Grade Epoxy Description: Master Bond EP3HTSMed is a one component, silver filled, electrically conductive epoxy system featuring high shear strength and good temperature resistance along with a fast cure schedu.. |