Polymer Property : Specific Gravity = 3.105 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.295 - 3.105 g/cc
2.295 - 3.105 g/cc
Parker Chomerics Tecknit Teckfip™ FIP-R Formed in Place Conductive Elastomer
Description: FIP-R is based on a very rugged pure silver particle. By using silver as the conductive medium, this compound offers great performance in terms of heat aged electrical conductive stabil..