Polymer Property : Specific Gravity = 5.20 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 5.20 g/cc
5.20 g/cc
DayGlo Phantom IPO-13 Invisible Pigment, Red
These materials have a yellowish or white color body under visible light and produce a bright vibrant color when exposed to an Ultra-Violet light source. Phantom pigments can be used for security an..
Specific Gravity 5.20 g/cc
5.20 g/cc
ASTM D792
Clariant Renol PA2SP0006 Nylon 6, Heavyweight Compound
Data provided by Clariant Masterbatches