Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 5.80 g/cc | 5.80 g/cc | Part A |
Epoxy Technology EPO-TEK® H81A Epoxy Material Description: A two component, gold-filled, electrically and thermally conductive epoxy designed for hybrid microelectronic and semiconductor packaging.Information Provided by Epoxy Technolo.. |