Physical Properties | Metric | English | Comments |
---|---|---|---|
Filament Diameter | 4.4 µm | 4.4 µm | |
Hexcel® HexTow™ IM9 Carbon Fiber HexTow™ IM9 carbon fiber is a continuous, ultrahigh performance, intermediate modulus, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be s.. |