Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 1000 cSt | 1000 cSt | Base Oil; ASTM D445 |
Nye Lubricants PG-1S Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 1000 cSt | 1000 cSt | Base Oil; ASTM D445 |
Nye Lubricants PG-2S Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 1000 cSt | 1000 cSt | Base Oil; ASTM D445 |
Nye Lubricants PG-3S Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 1000 cSt | 1000 cSt | Base Oil; ASTM D445 |
Nye Lubricants PG-4S Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 1000 cSt | 1000 cSt | Base Oil; ASTM D445 |
Nye Lubricants PG-8S Grease Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 1000 cSt | 1000 cSt | ASTM D445 |
ExxonMobil 1000 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Kinematic Viscosity at 40°C (104°F) | 1000 cSt | 1000 cSt | ASTM D445 |
ExxonMobil Extra Hecta Super Mineral Mobil Cylinder Oil Mobil Cylinder oils are extra high performance high viscosity oils designed for use in enclosed worm gears operating at moderate to high speeds and temperatures, and where heavy loads, slow speeds o.. |
|||
Kinematic Viscosity at 40°C (104°F) | 1000 cSt | 1000 cSt | ASTM D445 |
ExxonMobil Mobil Glygoyle 1000 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Kinematic Viscosity at 40°C (104°F) | 1000 cSt | 1000 cSt | ASTM D445 |
ExxonMobil 1000 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Kinematic Viscosity at 40°C (104°F) | 1000 cSt | 1000 cSt | ASTM D445 |
ExxonMobil Extra Hecta Super Mineral Mobil Cylinder Oil Mobil Cylinder oils are extra high performance high viscosity oils designed for use in enclosed worm gears operating at moderate to high speeds and temperatures, and where heavy loads, slow speeds o.. |
|||
Kinematic Viscosity at 40°C (104°F) | 1000 cSt | 1000 cSt | ASTM D445 |
ExxonMobil Mobil Glygoyle 1000 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Kinematic Viscosity at 40°C (104°F) | 1000 cSt | 1000 cSt | |
ConocoPhillips Inca® 1000 Oil, AGMA No. 8A Comp. Description: Conoco Inca Oil is a high-quality compounded lubricant recommended for use in heavily loaded industrial and automotive worm gears and bearings operating at moderate to high temperatures.. |
|||
Kinematic Viscosity at 40°C (104°F) | 1000 cSt | 1000 cSt | |
ConocoPhillips 1000 Gear Oil AGMA Lubricant No. 8AEP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |