Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 1080 cSt
1080 cSt
ASTM D-445
ConocoPhillips ANDEROL® PQ AA 1000 White Mineral Food Grade Gear Oil, ISO Grade 1000, SAE Gear Oil Grade 1000
Description: ANDEROL PQ AA Series Gear Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Gear..