Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ConocoPhillips ANDEROL® PQ AA 1000 White Mineral Food Grade Gear Oil, ISO Grade 1000, SAE Gear Oil Grade 1000

Category Fluid , Lubricant , White Mineral Oil (WMO)
Manufacturer ConocoPhillips
Trade Name ANDEROL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips ANDEROL® PQ AA 1000 White Mineral Food Grade Gear Oil, ISO Grade 1000, SAE Gear Oil Grade 1000.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ANDEROL PQ AA Series Gear Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Gear Oils provide excellent lubrication protection for gear sets, bearings, pumps and chain applications. The heavier viscosity grades can be used in worm gear applications with no harm to yellow metals. PQ food grade lubricants are approved, recommended and field tested by many OEMs in the food processing, baking, bottling, canning, meat processing and pharmaceutical industries. PQ food grade lubricants are listed by NSF International under “USDA Regulations, Proprietary Substances and Nonfood Compounds.”Information provided by ConocoPhillips.Anderol® is a registered trademark of The Anderol Company.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
60°F; ASTM D-1298
Viscosity Measurement 98
98
Viscosity Index; ASTM D-2270
Saybolt Viscosity at 100°F 5003 SUS
5003 SUS
ASTM D-2161
Saybolt Viscosity at 210°F 253 SUS
253 SUS
ASTM D-2161
Kinematic Viscosity at 40°C (104°F) 1080 cSt
1080 cSt
ASTM D-445
Kinematic Viscosity at 100°C (212°F) 54 cSt
54 cSt
ASTM D-445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 72.6 kg
160 lb (mass)
ASTM D-2783
Four Ball Wear 0.400 mm
0.0157 in
1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM D-4172
Thermal Properties Metric English Comments
Pour Point -10.0 °C
14.0 °F
ASTM D-97
Flash Point 200 °C
392 °F
ASTM D-92
Descriptive Properties Value Comments
Copper Corrosion 1B
3 hrs. at 100°C, ASTM D130
Rust Test Pass
ASTM D665A