Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 177 cSt | 177 cSt | Base Oil; ASTM D-445 |
ConocoPhillips Tacna® M5 Grease NLGI Grade 0 Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined.. |
|||
Kinematic Viscosity at 40°C (104°F) | 177 cSt | 177 cSt | Base Oil; ASTM D-445 |
ConocoPhillips Tacna® M5 Grease NLGI Grade 1 Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined.. |
|||
Kinematic Viscosity at 40°C (104°F) | 177 cSt | 177 cSt | Base Oil; ASTM D-445 |
ConocoPhillips Tacna® M5 Grease NLGI Grade 2 Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined.. |