Polymer Property : Kinematic Viscosity at 40°C (104°F) = 177 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 177 cSt
177 cSt
Base Oil; ASTM D-445
ConocoPhillips Tacna® M5 Grease NLGI Grade 0
Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined..
Kinematic Viscosity at 40°C (104°F) 177 cSt
177 cSt
Base Oil; ASTM D-445
ConocoPhillips Tacna® M5 Grease NLGI Grade 1
Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined..
Kinematic Viscosity at 40°C (104°F) 177 cSt
177 cSt
Base Oil; ASTM D-445
ConocoPhillips Tacna® M5 Grease NLGI Grade 2
Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined..