Polymer Property : Kinematic Viscosity at 40°C (104°F) = 20 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 20 cSt
20 cSt
Base Oil; ASTM D445
Nye Lubricants NPE-UC4 Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 40°C (104°F) 20 cSt
20 cSt
ExxonMobil Thermrex Series D-10
The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and ..
Kinematic Viscosity at 40°C (104°F) 20 cSt
20 cSt
ExxonMobil Thermrex Series F-43
The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and ..
Kinematic Viscosity at 40°C (104°F) 20 cSt
20 cSt
ASTM D445
ChevronTexaco ParaMount™ 1005 Paraffinic Process Oil
FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur..
Kinematic Viscosity at 40°C (104°F) 20 cSt
20 cSt
ExxonMobil Thermrex Series D-10
The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and ..
Kinematic Viscosity at 40°C (104°F) 20 cSt
20 cSt
ExxonMobil Thermrex Series F-43
The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and ..
Kinematic Viscosity at 40°C (104°F) 20 cSt
20 cSt
Base Oil
ConocoPhillips Grade 2 Calcium S Grease NLGI
Description: Conoco Calcium S Grease is a light, specialty calcium stearate thickened product that is used in the automotive assembly industry. It is amber in color and is used in applications where..
Kinematic Viscosity at 40°C (104°F) 20 cSt
20 cSt
ASTM D-445
ConocoPhillips ANDEROL® FGH 22 Synthetic Food Grade Hydraulic Fluid, ISO 22
Description: ANDEROL FGH Series Hydraulic Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA wh..