Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 20 cSt | 20 cSt | Base Oil; ASTM D445 |
Nye Lubricants NPE-UC4 Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 20 cSt | 20 cSt | |
ExxonMobil Thermrex Series D-10 The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and .. |
|||
Kinematic Viscosity at 40°C (104°F) | 20 cSt | 20 cSt | |
ExxonMobil Thermrex Series F-43 The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and .. |
|||
Kinematic Viscosity at 40°C (104°F) | 20 cSt | 20 cSt | ASTM D445 |
ChevronTexaco ParaMount™ 1005 Paraffinic Process Oil FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur.. |
|||
Kinematic Viscosity at 40°C (104°F) | 20 cSt | 20 cSt | |
ExxonMobil Thermrex Series D-10 The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and .. |
|||
Kinematic Viscosity at 40°C (104°F) | 20 cSt | 20 cSt | |
ExxonMobil Thermrex Series F-43 The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and .. |
|||
Kinematic Viscosity at 40°C (104°F) | 20 cSt | 20 cSt | Base Oil |
ConocoPhillips Grade 2 Calcium S Grease NLGI Description: Conoco Calcium S Grease is a light, specialty calcium stearate thickened product that is used in the automotive assembly industry. It is amber in color and is used in applications where.. |
|||
Kinematic Viscosity at 40°C (104°F) | 20 cSt | 20 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® FGH 22 Synthetic Food Grade Hydraulic Fluid, ISO 22 Description: ANDEROL FGH Series Hydraulic Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA wh.. |