Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 305 cSt | 305 cSt | ASTM D445 |
ChevronTexaco Drive Train Fluid HD, SAE 60 FeaturesChevron Drive Train Fluids HD are high performance lubricants designed for use in transmissions, final drives, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or Allison C4 .. |
|||
Kinematic Viscosity at 40°C (104°F) | 305 cSt | 305 cSt | ASTM D445 |
ChevronTexaco Ulti-Plex® NLGI 0 Greases EP FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The.. |
|||
Kinematic Viscosity at 40°C (104°F) | 305 cSt | 305 cSt | ASTM D445 |
ChevronTexaco Ulti-Plex® NLGI 1 Greases EP FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The.. |