Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 97 cSt | 97 cSt | Base Oil; ASTM D445 |
Nye Lubricants 182S (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 97 cSt | 97 cSt | ASTM D445 |
ExxonMobil Gargoyle Arctic 228 SHC 200 Series Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt.. |
|||
Kinematic Viscosity at 40°C (104°F) | 97 cSt | 97 cSt | |
ExxonMobil Mobil Clean 10W-40 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
Kinematic Viscosity at 40°C (104°F) | 97 cSt | 97 cSt | ASTM D445 |
ExxonMobil Gargoyle Arctic 228 SHC 200 Series Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt.. |
|||
Kinematic Viscosity at 40°C (104°F) | 97 cSt | 97 cSt | |
ExxonMobil Mobil Clean 10W-40 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
Kinematic Viscosity at 40°C (104°F) | 97 cSt | 97 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® 6100 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Kinematic Viscosity at 40°C (104°F) | 97 cSt | 97 cSt | |
ConocoPhillips Hydroclear® 10W-40 Super All Season and Super Motor Oil Description: Conoco Hydroclear Super All Season and Super Motor Oils, formulated with premium base stocks, lubricate domestic and imported passenger cars, sport-utility vehicles, light-duty trucks, .. |