Material Notes:
Description: Conoco Hydroclear Super All Season and Super Motor Oils, formulated with premium base stocks, lubricate domestic and imported passenger cars, sport-utility vehicles, light-duty trucks, minivans and high performance, late-model vehicles equipped with normally aspirated, turbocharged and supercharged gasoline engines. These advanced motor oils minimize engine deposits and wear and protect against high temperature oxidation, rust, corrosion and foaming. Hydroclear Super All Season Motor Oil viscosity grades SAE 5W-30 and 10W-30 carry ILSAC GF-3 energy-conserving credentials and are approved for API Service SL/EC. They carry the API certification mark for use in gasoline engines. Hydroclear Super All Season Motor Oil SAE 10W-40 and Hydroclear Super Motor Oil SAE 30 and 40 are approved for API Service SL. The SAE 30 grade is especially suited for use in small engines where a single-grade oil is recommended. These products, and especially the SAE 5W-30 grade, demonstrate exceptionally strong cold-temperature viscosity control compared to industry standards for appropriate grades. The control, measured by the Cold Cranking Simulator (CCS) and Mini-Rotary Viscometer (MRV TP-1), ensures excellent startability and prompt oil flow in the engine during very cold weather, thereby minimizing wear on critical engine components and resulting in longer engine life. In the appropriate viscosity grade, Hydroclear Super All Season and Super Motor Oils meet the performance requirements of these specifications: ILSAC GF-3 (5W-30 and 10W-30 only), API SLInformation provided by ConocoPhillips.
Physical Properties Metric English Comments
API Gravity 31 °
31 °
Viscosity Measurement 150
150
Viscosity Index
Saybolt Viscosity at 100°F 497 SUS
497 SUS
Saybolt Viscosity at 210°F 76 SUS
76 SUS
Kinematic Viscosity at 40°C (104°F) 97 cSt
97 cSt
Kinematic Viscosity at 100°C (212°F) 14.2 cSt
14.2 cSt
ASTM Color 3.5
3.5
Thermal Properties Metric English Comments
Pour Point -40.0 °C
-40.0 °F
Flash Point 216 °C
421 °F