Polymer Property : Kinematic Viscosity at 100°C (212°F) = 24.9 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 24.9 cSt
24.9 cSt
ASTM D445
ExxonMobil Mobil Almo 532
Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio..
Kinematic Viscosity at 100°C (212°F) 24.9 cSt
24.9 cSt
ASTM D445
ExxonMobil Mobil Almo 532
Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio..