Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 24.9 cSt | 24.9 cSt | ASTM D445 |
ExxonMobil Mobil Almo 532 Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio.. |
|||
Kinematic Viscosity at 100°C (212°F) | 24.9 cSt | 24.9 cSt | ASTM D445 |
ExxonMobil Mobil Almo 532 Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio.. |