Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 26.3 cSt | 26.3 cSt | Base Oil; ASTM D445 |
Nye Lubricants 760D (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 26.3 cSt | 26.3 cSt | Base Oil; ASTM D445 |
Nye Lubricants 345 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 26.3 cSt | 26.3 cSt | ASTM D445 |
ChevronTexaco Clarity® ISO 220 Synthetic Paper Machine Oil FeaturesChevron Clarity Synthetic Paper Machine Oils combine the unique ashless formulation of Chevron Clarity® Paper Machine Oils with the superior performance properties of polyalphaolefin (PAO) .. |