Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 163
163
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 205 cSt
205 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 26.3 cSt
26.3 cSt
Base Oil; ASTM D445
Evaporation Loss 0.10 %
0.10 %
24 hrs, 100C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 236
236
ASTM D217
Penetration P(60), 1/10 mm 268
268
ASTM D217
Oil Separation 1.7 %
1.7 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Recommended
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Recommended
Pour Point -45.0 °C
-49.0 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PAO
Gellant Type Silica(BL)