Kinematic Viscosity at 100°C (212°F) 54 cSt
54 cSt
Base Oil; ASTM D445
Nye Lubricants 327A (SO) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 54 cSt
54 cSt
Base Oil; ASTM D445
Nye Lubricants 731 (IG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 54 cSt
54 cSt
ASTM D-445
ConocoPhillips ANDEROL® PQ AA 1000 White Mineral Food Grade Gear Oil, ISO Grade 1000, SAE Gear Oil Grade 1000
Description: ANDEROL PQ AA Series Gear Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Gear..