Physical Properties Metric English Comments
Viscosity 1.33e+6 cP

@Shear Rate 12.0 1/s,
Temperature 275 °C
1.33e+6 cP

@Shear Rate 12.0 1/s,
Temperature 527 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm..