Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 147000 cP @Shear Rate 5000 1/s, Temperature 215 °C |
147000 cP @Shear Rate 5000 1/s, Temperature 419 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Viscosity | 147000 cP @Shear Rate 1000 1/s, Temperature 305 °C |
147000 cP @Shear Rate 1000 1/s, Temperature 581 °F |
DAM; ISO 11443 |
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |