Physical Properties Metric English Comments
Viscosity 147000 cP

@Shear Rate 5000 1/s,
Temperature 215 °C
147000 cP

@Shear Rate 5000 1/s,
Temperature 419 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging..
Viscosity 147000 cP

@Shear Rate 1000 1/s,
Temperature 305 °C
147000 cP

@Shear Rate 1000 1/s,
Temperature 581 °F
DAM; ISO 11443
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66  (Unverified Data**)