Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2.68 cP @Temperature 210 °C |
2.68 cP @Temperature 410 °F |
?=50 sec<sup>-1</sup> |
Gromax Evasin EV-3201V Ethylene-Vinyl Alcohol Copolymer Unmodified random Co-Polymer of [Ethylene-Vinyl alcohol], designed for therm-plastic processing into Sheets and Foils with high Oxygen and Aroma Barrier EffectInformation provided by Gromax Enterpri.. |