Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 2000 - 2500 cP

@Temperature 25.0 °C
2000 - 2500 cP

@Temperature 77.0 °F
at 20 rpm vibration
Permabond 2010 Cyanoacrylate, gap filling
PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy..
Viscosity 2000 cP

@Temperature 25.0 °C
2000 cP

@Temperature 77.0 °F
Of resin
Resin Technology Group TIGA 159 LV-UV Low Viscosity, Quick Gel UV Initiated, Flexible Epoxy Adhesive
Mix ratio 2 to 1 by volume.TIGA 159 LV-UV hybrid epoxy system is a low viscosity adhesive designed for small potting applications, bonding, laminating, sealing and structural repair applications whe..
Viscosity 2000 - 2800 cP

@Shear Rate 30.0 1/s,
Temperature 40.0 °C
2000 - 2800 cP

@Shear Rate 30.0 1/s,
Temperature 104 °F
P-3500 LCD MB7; 25 wt% polymer solution in DMAc
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)  (Unverified Data**)
Udel polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel P-3500 LCD MB series polymers are particularly well suited for the fabrication of porous ..
Viscosity 2000 cP

@Shear Rate 10.0 1/s,
Temperature 275 °C
2000 cP

@Shear Rate 10.0 1/s,
Temperature 527 °F
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY
Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th..