Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 24000 cP @Temperature -20.0 °C |
24000 cP @Temperature -4.00 °F |
MRV |
ExxonMobil Mobil Clean 20W-50 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
Viscosity | 24000 cP @Temperature -20.0 °C |
24000 cP @Temperature -4.00 °F |
MRV |
ExxonMobil Mobil Clean 20W-50 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
Viscosity | 24000 cP @Temperature -30.0 °C |
24000 cP @Temperature -22.0 °F |
MRV; ASTM D4684 |
ExxonMobil Mobil Delvac 10W-30 1300 Super Mobil Delvac 1300 Super 10W-30 and 15W-40 are extra high performance diesel engine oils that help extend engine life in the most severe on and off highway applications. The advanced chemistry of the.. |
|||
Viscosity | 24000 cP @Temperature -30.0 °C |
24000 cP @Temperature -22.0 °F |
MRV; ASTM D4684 |
ExxonMobil Mobil Delvac 10W-30 1300 Super Mobil Delvac 1300 Super 10W-30 and 15W-40 are extra high performance diesel engine oils that help extend engine life in the most severe on and off highway applications. The advanced chemistry of the.. |