ExxonMobil Mobil Clean 20W-50 Motor Oil

Category Fluid , Lubricant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Mobil Clean 20W-50 Motor Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. These oils protect against sludge and engine rust and corrosion under low-temperature operating conditions. Pour depressants and a viscosity index (VI) improver are included, where required, to provide the desired viscosity-temperature and low-temperature fluidity characteristics. Mobil Clean Oil is available in five multi-viscosity grades: SAE 5W-20, 5W-30, 10W-30, 10W-40, and 20W-50 Mobil Clean Oil 5W-20 has been introduced to meet the latest requirements of Ford and Honda. It meets the latest Ford Specification WSS-M2C 930-A. Mobil Clean Oil 5W-20, 5W-30 and 10W-30 contain friction-reducing additives. These viscosity grades are classified by the American Petroleum Institute (API) as "Energy Conserving" engine lubricants, and meet ILSAC GF-4.Mobil Clean Oil 5W-20 is recommended for vehicles which call for an API certified, 5W-20 viscosity grade engine oil such as 2001 and newer model year Ford automobiles, 1998 and newer model year Honda Accords, and 1996 and newer Honda Civics. It is also recommended for 2005 Chrysler vehicles where a 5W-20 is recommended. This unique viscosity grade should be used only in automobiles that require a 5W-20 lubricant and it is not recommended for use in other vehicles. Mobil Clean Oil 5W-30 and Mobil Clean Oil 10W-30 are recommended for gasoline fueled automobiles and light duty trucks requiring an API SM, SL, SJ or SH product. They meet ILSAC GF-4 (Starburst Certification Symbol). Mobil Clean Oil 10W-40 is recommended for gasoline fueled automobiles and light duty trucks where a higher viscosity oil is preferred or recommended and where an API SM, SL, SJ or SH product is required. Mobil Clean Oil 20W-50 is recommended for high-performance engines found in race and rally driving. It has a higher viscosity reserve which provides engines with full protection under higher operating speeds, temperatures, and other adverse conditions. This product is also recommended for gasoline fueled automobiles and light trucks where a higher viscosity oil is preferred or recommended. Before using a Mobil Clean Oil, consult the owners manual of the vehicle for the manufacturers recommended viscosity grade and API Service Classification.
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
API Gravity 27.4 °
27.4 °
Viscosity 8200 cP

@Temperature -15.0 °C
8200 cP

@Temperature 5.00 °F
CCS
24000 cP

@Temperature -20.0 °C
24000 cP

@Temperature -4.00 °F
MRV
Viscosity Measurement 124
124
Index
Kinematic Viscosity at 40°C (104°F) 162 cSt
162 cSt
Kinematic Viscosity at 100°C (212°F) 18.1 cSt
18.1 cSt
Thermal Properties Metric English Comments
Pour Point -27.0 °C
-16.6 °F
Flash Point 200 °C
392 °F
Descriptive Properties Value Comments
Energy Conserving no