Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 240000 - 240000 cP @Temperature 250 - 250 °C |
240000 - 240000 cP @Temperature 482 - 482 °F |
Average value: 240000 cP Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Viscosity | 240000 - 240000 cP @Shear Rate 1000 - 1000 1/s |
240000 - 240000 cP @Shear Rate 1000 - 1000 1/s |
Average value: 240000 cP Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |